Kinetic oxidations of phenol by piroluzit containing minerals

Authors:
O. V. Cheremisina1
M. A. Sulimova2
D. E. Chirkst3
About authors
  • 1 — Ph.D., Dr.Sci. associate professor National Mineral Resources University (Mining University)
  • 2 — post-graduate student National Mineral Resources University (Mining University)
  • 3 — Ph.D., Dr.Sci. professor National Mineral Resources University (Mining University)
Date submitted:
2012-09-01
Date accepted:
2012-11-08
Date published:
2013-04-29

Abstract

The kinetics parameters of phenol oxidation by MnO2 on the surface of iron-manganese nodules at pH = 5,5±0,5 at temperature region from 293 till 353 K was described in this paper. The oxidation reaction runs by second order on phenol. At temperature region from 293 till 353 K the limited stage is chemical reaction. The activation energy of oxidation on the surface of iron-manganese nodules is equal 6,65 kJ/mol, and it is less than it’s one for oxidation on MnO2 surface (42,0 kJ/mol). The oxidation products are hydrohinon and less than 10 pier. % p-benzohinon.

Область исследования:
(Archived) Without section
Keywords:
phenol kinetics of oxidation interfacial reactions hydrohinon benzohinon
Funding:

None

Go to volume 202

References

  1. Lure J.J. The chemical analysis of industrial sewage / J.J.Lure, A.I.Rybnikova. Мoscow, 1974. 271 p.
  2. Serikov N.F. Water management of ferrous metal-lurgy factories. Мoscow, 1973. 408 p.
  3. Matocha Ch.J. Role of Mn(III) in Oxidation of Soil Organic Matter / Ch.J.Matocha, D.L.Sparks, J.E.Amonette, R.K.Kukkadapu // Soil Science Soc. of Amer.J. 2001. Vol. 65. N 1. P.58-66.
  4. Ukrainczyk L. Oxidation of phenol in acidic aque-ous suspensions of manganese oxides / L.Ukrainczyk, M.B.McBride // Clays and Clay Minerals. 1992. Vol. 40. N 2. P.157-166.

Similar articles

Causes and significance of inflections in hydrocyclone efficiency curves
2013 E. E. Andreev, V. V. Lvov, A. V. Fadina
Study of the corrosion stability of some materials in the titanium (II) and (III) chloride melts
2013 I. I. Ivanov, O. A. Dubovikov, L. V. Grigoreva, A. A. Kuzhaeva, P. V. Zgonnik
Study of the separation process dispersed nonuniform systems for conditioning bauxite
2013 V. M. Sizyakov, O. A. Dubovikov, N. V. Nikolaeva
Highly basic bauxite agglomerates
2013 V. A. Utkov, O. V. Zyryanova, M. G. Yakovlev
Investigation of the colored organic compounds behavior in aluminate liquors during electrolysis treatment
2013 Yu. A. Zaitsev, E. V. Tikhonova, E. V. Sizyakova
Control and management e of electric arc ratio in ore-smelting furnace
2013 A. P. Suslov, N. I. Koteleva, Yu. L. Zhukovskii, V. V. Vasilev