EFFECT OF CHALK THERMAL TREATMENT MODE ON ITS STRENGTH

Article preview

Natural chalk is characterized by a fine-grained structure. The processing of chalk in conditions traditional for calcium carbonate baking is accompanied by its almost destruction and the formation of a huge amount of dust. The paper presents strength characteristics of chalk and chalky stone baking obtained with different temperature-time conditions of heating the raw material to a temperature of 450-600 °C. The uniaxial compression method was used to determine the strength depending on variable factors. Based on the experimental data, a model was constructed that determines the dependence of chalk strength on time and heating temperature. In the temperature range of 450-600 °C, the strength of chalk stone increases with increasing temperature and decreases with the increasing heating rate. In the process of isothermal heating, several factors will immediately affect the strength of a chalky stone: the formation and growth of calcite crystals, the evaporation of water, and the agglomeration of calcite grains. With an increase in the heating temperature from 450 to 600 °C, the average size of the crystals significantly increases and crystals with an estimated size of more than 4 microns are detected. An increase in the size of crystals is associated with an increase in their growth rate. The agglomeration of grains occurs at a temperature of 600 °C.

How to cite: Lipin V.A., Trufanov D.A. EFFECT OF CHALK THERMAL TREATMENT MODE ON ITS STRENGTH // Journal of Mining Institute. 2019. Vol. 236. p. 210. DOI: 10.31897/PMI.2019.2.210
Metallurgy and concentration
  • Date submitted
    2018-05-06
  • Date accepted
    2018-07-17
  • Date published
    2018-10-25

OBTAINING INTERMETALLIC COMPOUNDS IN Al–Ti–Zn SYSTEM

Article preview

Binary intermetallic compounds – titanium aluminides (TiAl, Ti 3 Al) – when added to the alloys, significantly increase their strength and special properties. The most promising direction to produce intermetallic compounds are mechanochemical technologies, including mechanical alloy building. Mechanical alloying makes it possible to introduce much smaller particles into the metal matrix than can be achieved using standard powder metallurgy technologies. In addition to mechanical synthesis, aluminum-based intermetallic compounds were produced by self-propagating high-temperature synthesis (SHS) of solid chemical compounds. The synthesis was carried out according to a multistage scheme: preparation of titanium and aluminum powder, mixing; synthesis of the Al 3 Ti intermetallic compound by the SHS method in vacuum followed by mechanical activation of stoichiometric charges. The aim of the research was to study the dynamics of the development of nanodispersed phases in the process of synthesis during mechanical alloying. The power absorbed by the unit mass of the material for different processing times of the charge was calculated. When the level of the specific power (dose) of mechanical treatment was 3.5 kJ/g, the maximum content of intermetallic compound in the resulting material was achieved. Based on calculations and the data obtained during X-ray phase analysis, the dependence of the change in the content of ternary intermetallic compounds in the final product on the absorbed power was determined. As a result of the studies using raster electron microscopy and X-ray analysis, it was found that mechanical alloying of nanostructured intermetallic compounds Ti 4 ZnAl 11 and Ti 25 Zn 9 Al 66 with the size of nanodisperse phases less than 12 nm in the Al–Ti–Zn system, the weight ratio of proportion of the latter reaches 74 %.

How to cite: Kaminskii V.V., Petrovich S.A., Lipin V.A. OBTAINING INTERMETALLIC COMPOUNDS IN Al–Ti–Zn SYSTEM // Journal of Mining Institute. 2018. Vol. 233. p. 512. DOI: 10.31897/PMI.2018.5.512
Metallurgy and concentration
  • Date submitted
    2017-10-31
  • Date accepted
    2018-01-01
  • Date published
    2018-04-25

Peculiarities of formation and growth of nanodispersed intermetallic strengthening inclusions in rapidly-solidified alloys of Al–Mg–Zr–X-system

Article preview

The paper is devoted to the influence of the fourth element on the microstructure of the rapidly-solidified alloys of the Al–Mg–Zr-system. Alloys were additionally doped with high-melting-point metals Ti, Hf, W, and Nb. In the structure of all samples in the immediate area of the cooled surface, uniformly distributed intermetallic inclusions of several nanometers in size were detected. Such a structure can be represented as a dispersion-strengthened composite. A quantitative metallographic analysis was carried out to quantitatively describe the structure of the obtained particles of the cooled melt. The obtained rapidly-solidified alloys can be described as dispersion-strengthened composite materials with the aluminum-magnesium alloy matrix and the intermetallic particles strengthener. Depending on the alloying component, these particles differ in shape (spheres, plates, agglomerates) and in size (from 200 nm when alloying with Hf and W up to 1.2-1.5 μm with Ti and Nb alloying). The X-ray phase analysis (XPA) showed that in the studied alloys of the Al–5Mg–1.2Zr–(0.5÷2.0)X-system, high cooling rates of melts lead to the formation of new intermetallic compounds that are absent in equilibrium systems. The example of an alloy with hafnium additive shows that an increase in the content of the alloying component (from 0.5 to 2 % by mass) leads to an increase in the volume ratio of intermetallic inclusions (from 5 to 12.8 %). At the same time, their shape and average size remain unchanged. The additional alloying component will improve the mechanical characteristics of aluminum alloys by increasing the recrystallization threshold of a rapidly-solidified alloy.

How to cite: Budelovskii D.I., Petrovich S.Y., Lipin V.A. Peculiarities of formation and growth of nanodispersed intermetallic strengthening inclusions in rapidly-solidified alloys of Al–Mg–Zr–X-system // Journal of Mining Institute. 2018. Vol. 230. p. 139. DOI: 10.25515/PMI.2018.2.139
Without section
  • Date submitted
    2012-09-09
  • Date accepted
    2012-11-23
  • Date published
    2013-03-01

Microalloying of aluminum as the method оf changing properties of powder oxidation film

Article preview

The method of x-ray electronic spectroscopy investigated influence of strontium, bismuth  and a lead and tin alloy on structure of superficial films of powders of oxide of aluminum. It is established that alloying additives are surface-active substances and concentrate mainly in a blanket, partially being oxidized together with aluminum. Being formed superficial films have impact on consumer properties of aluminum  powders.

How to cite: Baimakov A.Y., Petrovich S.Y., Seitenov R.A., Lipin V.A., Shakhmin A.L. Microalloying of aluminum as the method оf changing properties of powder oxidation film // Journal of Mining Institute. 2013. Vol. 202. p. 278.