Processes of oxidation of impurities of metal concentrate of radio-electronic scrap
Authors:
About authors
- G.V. Plekhanov Saint Petersburg Mining Institute
Abstract
The study was carried out in order to find technological conditions that allow anodic dissolution of metal concentrate of radio-electronic scrap without difficulties caused by anode passivation. The thermodynamic probability of sufficiently complete oxidation of impurities included in the metal concentrate was established. The composition of refining slag allowing to bind oxidized impurities in slag is selected. Time dependence of oxidation of impurities by air due to application of radial-axial tuyere is shown. It is indicated that for 15min of blowing it is possible to prepare the metal-concentrate alloy for successful anodic dissolution in sulfuric acid electrolyte.
Область исследования:
(Archived) Without section
Funding:
None
Similar articles
Investigation of silver selenide behavior in aqueous solutions
2006 G. V. Petrov, A. M. Belenkii, A. Ya. Boduen
Low-temperature desiliconization of aluminate solutions on activated inoculants
2006 V. N. Brichkin, E. V. Sizyakova, R. S. Gordeev
Thermodynamic bases of recrystallization of alumina production precipitates with participation of gas phase
2006 V. N. Brichkin, A. V. Tsybizov, R. S. Gordeev
Model of technology of limestone roasting in a shaft kiln
2006 I. N. Beloglazov, V. O. Golubev, O. V. Ziyazitdinova