G. A. Senkin
G. A. Senkin

Co-authors

Articles

Article
  • Date submitted
    1980-09-03
  • Date accepted
    1980-11-05

Development of wear resistance scale for machined and tool materials

Article preview

The existing methods and devices for determining the wearability of various materials when rubbing against fixed and unfastened abrasive particles do not take into account the loss of cutting ability of abrasive grains, changes in the sliding speed during the experience and other factors affecting the accuracy and stability of the results obtained ...

How to cite: Senkin G.A. Development of wear resistance scale for machined and tool materials // Journal of Mining Institute. 1981. Vol. 86. p. 65.
Article
  • Date submitted
    1975-08-20
  • Date accepted
    1975-10-11

Use of synthetic superhard material Elbora-B in rock-destroying drilling tools

Article preview

Successes in the synthesis of new superhard materials, in particular, cubic boron nitride (elboron), which has increased heat resistance compared to natural diamond and hard alloy (respectively 1.8 and 1.6 times) and chemical inertness to ferrous compounds, opened wide opportunities to expand and improve the raw material base for the manufacture of drilling rock-destroying tools ...

How to cite: Shamshev F.A., Senkin G.A., Gorshkov L.K. Use of synthetic superhard material Elbora-B in rock-destroying drilling tools // Journal of Mining Institute. 1976. Vol. 71. Iss. 2. p. 16-19.
Article
  • Date submitted
    1972-07-12
  • Date accepted
    1972-09-05

Evaluation of the possibility of reinforcing drilling tools with synthetic superhard materials in standard binder-matrixes

Article preview

Standard tungsten-cobalt carbide bonds, depending on their hardness and purpose, are produced by cold (No. 3, 20-25 HRC, and No. 4, 30-35 HRC) and hot (No. 5, 50-55 HRC) pressing methods. Temperatures of sintering of bond-matrixes vary in the range from 1150 (No. 3) to 1350°C (No. 5) and in a reducing medium do not lead to the appearance of noticeable traces of graphitization. or loss of mechanical strength in perfect single crystals of natural diamond.

How to cite: Gorshkov L.K., Sumaneev N.N., Senkin G.A. Evaluation of the possibility of reinforcing drilling tools with synthetic superhard materials in standard binder-matrixes // Journal of Mining Institute. 1973. Vol. 66. Iss. 1. p. 102-108.